Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790-95 |
Multibase Multi-Pro® 1602 S Black Polypropylene Data provided by Multibase. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | Secant @ 1% strain; ASTM D790 |
Ineos H28E-00 Polypropylene Homopolymer, Antistatic Grade H28E-00 is an antistated, controlled rheology polypropylene homopolymer. It is designed for injection molding applications that require improved impact. This material meets the Food and Drug.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 530A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 550E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Flexural Modulus | 1.379 - 1.792 GPa | 200.0 - 259.9 ksi | ASTM D790 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Flexural Modulus | 1.379 - 1.792 GPa | 200.0 - 259.9 ksi | ASTM D790 |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | ASTM D790 |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Modulus | 1.379 GPa | 200.0 ksi | I.B., TAN, 0.5 in/min; ASTM D790 |
Solvay Engineered Polymers SEQUEL® E2200 TPO
(discontinued **) Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This pro.. |