Polymer Property : Flexural Modulus = 2.10 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0145 GPa
2.10 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 6001 BLK
TPE A 6001 is designed for gasket seals, rotational valves, and electrical applications as well as low friction applications. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.