Polymer Property : Flexural Modulus = 194.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.344 GPa
194.9 ksi
ASTM D790
Eastman Tenite 307A4000015 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Flexural Modulus 1.344 GPa
194.9 ksi
ASTM D790
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel..
Flexural Modulus 1.344 GPa
194.9 ksi
ASTM D790
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 1.344 GPa
194.9 ksi
ASTM D790
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..