Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.336 GPa | 193.7 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH042V Polypropylene, Homopolymer, Extrusion, Sheet COPYLENE™ CH042V is a polypropylene homopolymer resin often used in extrusion applications. Replacement alternative to Pro-fax® HL561KInformation provided by Phillips 66. |