Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
  AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Techmer ES Electrablend® PPS 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF50 50% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Clariant Renol PA213G50 Nylon 6, 50% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM Test |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH
(di AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Flexural Modulus | 13.1 GPa | 1900 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-4133 V0 Z Polyphthalamide (PPA), Dry
(discontinued **) Amodel AFA-4133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |