Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.309 GPa | 189.9 ksi | chs 0.05 in/min; 1% secant; ASTM D790 |
Diamond Polymers NPP30-3500G Homopolymer Polypropylene Granules Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 1.309 GPa | 189.9 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Flexural Modulus | 1.309 GPa | 189.9 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |