Polymer Property : Flexural Modulus = 189.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.303 GPa
189.0 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene
Mineral filled PP compound for interior automotive applications. Product meets GMP PP 056 and EBG-M4 D605-A specifications. Ash is 10%.Data provided by Multibase.