Flexural Modulus | 1.30 GPa | 189 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AS66K-01 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Polimeri Europa Eraclene® MS 80 U High Density Polyethylene - Injection Molding Eraclene MS 80 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This grade has a narrow molecular weight distribution and a hig.. |
|||
Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Flexural Modulus | >= 1.30 GPa | >= 189 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1532B (YD50G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.30 GPa | >= 189 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1401D (Q30P) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding PA 66, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | DIN 53452; ASTM D790 |
Kolon Kopa® KN151 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Solvay TECHNYL® A 402H1 Natural PA66, Conditioned Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 3 points and 2 mm/min; ISO 178 |
Styron INSPIREâ„¢ TF0808S(U) Polypropylene TF0808S(U) is a talc filled PP exhibiting high impact resistance and a high stiffness. It is particularly well suited for low wall thickness bumper skins. INSPIRE TF0808S for painted parts INSPIRE .. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Solvay TECHNYL® A 208F PA66, Conditioned Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 2mm/min; ISO 178 |
Borealis BA390TF Polypropylene Copolymer BA390TF is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA390TF is recommended for foam extrusion, or thermoforming.Inform.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Flexural Modulus | >= 1.30 GPa | >= 189 ksi | ASTM D790 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
Eastman Tenite 572E3720012 Cellulose Acetate Butyrate, Clear, Trsp Applications:FilmsProfilesSheetProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a wa.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 1% secant, 0.5 in/min; ASTM D790B |
ExxonMobil PP7033E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate.Availability: North America and Asia Pacific Featu.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam MX05075 PP, Flame Retardant, Injection Molding Starflam MX05075 is an Unfilled Halogen Free Flame Retardant PP Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO R178 |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
Braskem H 107 Coating Polypropylene Description: H 107 is a ultra-high melt flow rate additivated homopolymer used for general purposes. Designed for extrusion coating. This product exhibits excellent processability, good melt stabili.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
Buckeye Polymers BP Flex D9010 UC85 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, Conditioned Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 608 Nylon 6/12, Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPC 15000 Polypropylene Copolymer Information provided by Polykemi AB |