Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.28 GPa | 185 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
PolyMirae Moplen 341R Injection Molding Grade Polypropylene Moplen RP341R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP341R is a random copolymer particularly suitable for injecti.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
PolyMirae Moplen RP340R Injection Molding Grade Polypropylene Moplen RP340R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340R is a random copolymer particularly suitable for injecti.. |
|||
Flexural Modulus | 1.27 - 1.76 GPa | 185 - 256 ksi | Average value: 1.47 GPa Grade Count:5 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Hyosung Topilene HJ646 PP HJ646 Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Hyosung Topilene J740 PP J740 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporation.. |
|||
Flexural Modulus | 1.27 GPa @Thickness 6.40 mm |
185 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790B |
Ineos L12Z-01 Polypropylene Impact Copolymer Grade L12Z-01 is a nucleated and antistatic polypropylene copolymer with a medium melt flow rate that provides an excellent balance of stiffness and impact. It is especially formulated to help provi.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Tangent-Method; ASTM D790 |
Ineos T50-400 HDPE T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D760 |
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
LG Chemical SEETEC PB283 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
LG Chemical SEETEC PH162 HDPE Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
LG Chemical SEETEC PM360 HDPE Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | 5 mm/min; ISO 178 |
Gromax BTE90-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Flexural Modulus | 1.27 GPa @Thickness 6.40 mm |
185 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | secant; ASTM D790 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | |
Shinil Chemical SHINSTAT PETG Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6105JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityWide service temperatureHigh rigidityGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drinks, bottles, pallet, garbage bins, .. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790-90 |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 3255 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers good impact strength, resistance to warpage, and stiffness. This product meets the Food and Drug Administration requ.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D-790 |
Bapolene® 4072 Polypropylene, Injection Grade Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Asia Technology Pioneers CAP 501 PP Nanocomposite Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Lene™ H6140B High Density Polyethylene Blow Molding Key Characteristics:Good processabilityHigh stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthExcellent appearanceOdorlessSafe for food contactGood pri.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem F013M Homopolymer Polypropylene Description: General PurposeApplications: Suggested Uses Include Strapping, ProfilesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food an.. |