Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.74 GPa | 1848 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Flexural Modulus | 12.74 GPa | 1848 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Flexural Modulus | 12.74 GPa | 1848 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
Flexural Modulus | 12.74 GPa | 1848 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Flexural Modulus | 12.74 GPa | 1848 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Flexural Modulus | 12.74 GPa | 1848 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |