Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.54 GPa | 1819 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |
|||
Flexural Modulus | 12.54 GPa | 1819 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |