Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
PolyOne Stat-Tech™ PS-18CF/000 CM Black Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinu Preliminary Data SheetDescription/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | Lengthwise; ASTM D790 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Flexural Modulus | 12.4 - 13.1 GPa | 1800 - 1900 ksi | ASTM D790 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 12.41 GPa | 1800 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
Flexural Modulus | 12.41 GPa | 1800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific) LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific) LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Flexural Modulus | 12.41 GPa | 1800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS LNP* THERMOCOMP* ZF0049 is a compound based on PPE+PS resin containing 20% Glass Fiber. Added feature of this material is: Flame Retardant. |
|||
Flexural Modulus | 12.41 GPa | 1800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RV008S PA 66 (Asia Pacific) LNP* Verton* RV008S is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 464 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Flexural Modulus | 12.4 GPa | 1800 ksi | ASTM D790 |
PolyOne Edgetek® AM 33 GF/000 L HS Black Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Heat StabilizedBlackEnhanced LubricationGlass Fiber ReinforcedInformation provided by PolyOne Corporation. |