Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.24 GPa | 180 ksi | Tangent; ASTM D790 |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 600 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | Tangent; ASTM D790 |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D 790 |
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin 19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH085 Polypropylene, Homopolymer, Cast Film COPYLENE™ CH085, a controlled rheology polypropylene homopolymer resin, is used in injection molding and cast film extrusion applications. Applications: Bags & Pouches, Stationery Film, Stretch Wra.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790B |
Ineos N05G-00 Polypropylene Impact Copolymer Grade N05G-00 is a general purpose high impact copolymer polypropylene for injection molding applications. It offers a superior balance of stiffness and impact strength as compared to competitive im.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790A |
Ineos L70Z-01 Polypropylene Impact Copolymer L70Z-01 is a nucleated and antistatic high flow polypropylene medium impact copolymer for injection molding applications. This product meets the requirements of the U.S. Food and Drug Administration.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
Techmer ES HiFill® HDPE TM25 25% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4101M Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101M is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 5 mm/min, tangent; ASTM D790 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 5 mm/min, tangent; ASTM D790 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 55600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Food Pails.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790B |
ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, .. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BA50-100 Blow Molding Resin Product Description: BA50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | Secant @ 1% strain; ASTM D790 |
Bapolene® PP5062 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin offers a superior balance of stiffness and impact strength. This product meets the FDA requirements of .. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | Secant @ 1% strain; ASTM D790 |
Bapolene® PP5072 Polypropylene, Injection Grade Bapolene PP 5072 is a multipurpose, high flow impact copolymer with excellent color and processability. This resin also exhibits a superior balance of stiffness and impact strength. This product m.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem CP1200B Homopolymer Polypropylene Description: General PurposeApplications: Suggested Uses Include CompoundingThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug A.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4015F2 Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the r.. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BC50-100 Sheet Extrusion and Blow Molding Resin
(discontinued **) BC50-100 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Information provided by ExxonMobil .. |
|||
Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |