Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.130 GPa | 18.9 ksi | ISO 178 |
Polimeri Europa Riblene® MM 20 Low Density Polyethylene - Injection Molding Riblene MM 20 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 are characterized by a high flexibility.Main Applications: Riblene MM 20 is suitable for injecti.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | ISO 178 |
Polimeri Europa Riblene® MM 20 R Low Density Polyethylene - Injection Molding Riblene MM 20 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 R are characterized by a high flexibility.Main Applications: Riblene MM 20 R is suitable for i.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | ISO 178 |
Polimeri Europa Riblene® MP 20 Low Density Polyethylene - Injection Molding Riblene MP 20 is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MP 20 are characterized by a high flexibility.Main Applications: Riblene MP 20 is suitable for injecti.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | ASTM D790 |
Rotuba H2 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD801AU PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP821U PPE-TPE (Asia Pacific) UV stabilized, halogen free Flexible Noryl injection molding grade for overmolding applications such as plugs, strain relief's, and connectors. Good color stability after UV weathering per ASTM D445.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | ASTM D638 |
Arkema Group LOTADER® TX 8030 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER TX 8030 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER TX 8030 is an adhesive designed for extrusion coating .. |
|||
Flexural Modulus | 0.130 GPa | 18.9 ksi | ASTM D790 |
LATI LATISTAT 48/9900-03 Ethylene Vinyl Acetate (EVA) Base Conductive Plastic
(Unverified Data**) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |