Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 120 GPa | 17400 ksi | |
SGL Carbon Group SIGRAFIL C® in 250°F Epoxy 60% fiber volumeInformation provided by SGL Carbon Group |
|||
Flexural Modulus | 120 GPa | 17400 ksi | 0° |
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape Not Supported 150 g/m2 Information provided by HexCel |