Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.92 GPa | 1729 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 11.92 GPa | 1729 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 (Asia Pacific) LNP VERTON* RVL28 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Easy Molding. |