Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 11.72 GPa | 1700 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
PolyOne Edgetek® NL-20CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 11.72 GPa | 1700 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Techmer ES HiFill® PA12 GF50 L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Techmer ES HiFill® PET GF/M40 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Ensinger Tecapeek® XP-114 Compression Molded PEEK Compound, 40% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
Ashley Polymers Ashlene® E128 PET Polyester, 45% Glass Reinforced PET Polyester, economy grade with 45% glass reinforcement.Data provided by the manufacturer |
|||
Flexural Modulus | 11.7 - 13.1 GPa | 1700 - 1900 ksi | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Flexural Modulus | 11.7 - 12.4 GPa | 1700 - 1800 ksi | |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Flexural Modulus | 11.7 - 13.1 GPa | 1700 - 1900 ksi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Flexural Modulus | 11.72 GPa | 1700 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 (Asia Pacific) LNP* THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 11.7 GPa | 1700 ksi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |