Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.09 GPa | 158 ksi | Chord; 2 mm/min; ISO 178 |
Mytex Polymers AS43L-01 Polypropylene, Rubber modified, Compounded Description: AS43L-01 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key.. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem HA 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | ASTM D790 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | Secant, 0.079 in/min; ISO 178 |
ExxonMobil Exxtral™ H1025W Performance Polyolefin Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive.. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | ASTM D790 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | ASTM D790 |
Clariant Renol PPSP0004 Polypropylene, Random Copolymer Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE) Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme.. |
|||
Flexural Modulus | 1.09 GPa | 158 ksi | ASTM D-790 |
Bapolene® 3039U Polyethylene, Rotational Molding Grade Bapolene 3039U is a hexene linear low density polyethylene designed to provide superior impact resistance. It contains a UV-stabilization package and complies with US FDA 21CFR177.1520.Applications.. |