Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LATI LARPEEK 10 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH
&n AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Thermocomp® EF-1006 EM Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WFL28 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WFL28 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific) LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS (Europe-Africa-Middle East) LNP* Thermocomp* OF-1006 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UCF22S PPA LNP* Thermocomp* UCF22S is a compound based on Polyphthalamide resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE003E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE003E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | dry; ISO 178 |
DSM Akulon® K224-G8 PA6-GF40 40% Glass Reinforced |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 247 SAN, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |
|||
Flexural Modulus | 10.8 GPa | 1570 ksi | ASTM D790 |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |