Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.46 GPa | 1517 ksi | ISO 178 |
Polyplastics Duranex® CN7130 Polybutylene Terephthalate (PBT), Low friction, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |