Mechanical Properties Metric English Comments
Flexural Modulus 10.345 GPa
1500.4 ksi
ASTM D-790
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
Flexural Modulus 10.345 GPa
1500.4 ksi
ASTM Value
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. ..