Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.103 GPa | 15.0 ksi | ASTM D790 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Flexural Modulus | 0.103 GPa | 15.0 ksi | 2% Secant; ASTM D790 |
Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be.. |
|||
Flexural Modulus | 0.103 GPa | 15.0 ksi | ASTM D790 |
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien.. |