Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.31 GPa | 1495 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON EX99689C PEI LNP* STAT-KON* EX99689C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Flexural Modulus | 10.31 GPa | 1495 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Flexural Modulus | 10.31 GPa | 1495 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific) LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Flexural Modulus | 10.31 GPa | 1495 ksi | ISO 178 |
Polyplastics Duranex® CN7030 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |