Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.2732 - 19.3053 GPa @Temperature -40.0 - 121 °C |
1490.02 - 2800.04 ksi @Temperature -40.0 - 250 °F |
Average value: 14.4 GPa Grade Count:3 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |