Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyOne LubriOne™ ATT-000/5T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyMirae Moplen RP370G Blow Molding Grade Polypropylene Moplen RP370G is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP370G is a copolymer particularly suitable for blow molding applicat.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 301 EXT Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Chevron Phillips Marlex® HMN 4550 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520. High stress crack resistance, impact strength, and warpage resistance.Data provided by the manufacturer |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9001-16H , 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ASTM D790 |
Flint Hills 13T25A Random Copolymer Polypropylene Features: Excellent clarity, blush resistant and good flexural modulus. Product does not contain animal derived components.Applications: Injection Molded - Lab ware, food packaging and medical. .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Olsen Stiffness; ASTM D747 |
Global B-6200 High Density Polyethylene Description-suitable for high quality blow molding, provides excellent surface glossiness in combination w/ outstanding environmental stress cracking resistanceApplications-cosmetics bottles, shampo.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem HD 7255 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | |
Total PPH 3727WZ Polypropylene, Injection Molding Grade Fina’s new HIGH PERFORMANCE injection molding gradeBalanced Properties - Fina 3727WZ strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an a.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ISO 178 |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | |
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3802 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Asia Technology Pioneers CAP 502 PP Nanocomposite Description: CAP502 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D-790 |
Axiall 3801 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM-D790 |
Polyram RamOfin PPC300S4BK10 Polypropylene, 20% Glass beads 20% glass beads reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.03 - 3.10 GPa | 149 - 450 ksi | Average value: 1.89 GPa Grade Count:27 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
SCG Chemicals EL-Lene™ H5211PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |
|||
Flexural Modulus | 1.03 GPa | 149 ksi | ASTM D790 |
LG Chemical LUTENE-H ME8000 HDPE Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated.. |