Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.25 GPa | 1487 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |