Flexural Modulus 1.01 GPa
146 ksi
1% SEC, 0.05 in/min; ASTM D790
Solvay Engineered Polymers INDURE™ E1500 HG TPO  (discontinued **)
Description: INDURE™ E1500 HG is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material..
Flexural Modulus 1.01 GPa
146 ksi
1% SEC, 0.05 in/min; ASTM D790
Solvay Engineered Polymers INDURE™ E1600 TPO  (discontinued **)
Description: INDURE™ E1600 is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material is..
Flexural Modulus 1.01 GPa
146 ksi
12.5 mm/min; ASTM D790
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a..
Flexural Modulus 1.01 GPa
146 ksi
2% secant; ASTM D790-02
Ipiranga Petrochem GF 5250 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Flexural Modulus 1.01 GPa
146 ksi
1% secant, 0.05 in/min.; ASTM D790
ExxonMobil PP7035E4 Impact Copolymer
Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional ..
Flexural Modulus 1.01 GPa
146 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DMDB-7950 NT 7 High Density Polyethylene Resin
DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo..
Flexural Modulus 1.01 GPa
146 ksi
Dow HDPE 08454N High Density Polyethylene
DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wi..
Flexural Modulus 1.01 GPa
146 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE)
Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household..
Flexural Modulus 1.01 GPa
146 ksi
Dow HDPE 65053N High Density Polyethylene
DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen..
Flexural Modulus 1.01 GPa
146 ksi
ISO Data
BASF Ultramid® 8202CQ PA6 (Conditioned)
Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme..
Flexural Modulus 1.01 GPa
146 ksi
ASTM D790
Multibase Multi-Flam™ 0801 PP Polypropylene