Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.90 GPa | 1440 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Flexural Modulus | 9.93 GPa | 1440 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 9.96 GPa | 1440 ksi | ASTM D790 |
Plenco 50030 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Flexural Modulus | 9.92 GPa | 1440 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant. |
|||
Flexural Modulus | 9.93 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
Flexural Modulus | 9.93 GPa | 1440 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Flexural Modulus | 9.94 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Flexural Modulus | 9.92 GPa | 1440 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific) LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 9.96 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXY PA 66 LNP* Thermocomp* RF006XXY is a compound based on Nylon 66 containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific) LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Flexural Modulus | 9.94 GPa | 1440 ksi | ISO 178 |
Polyplastics Duranex® CN5330 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178-93 |
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 42H-BKDX9 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO Data |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO Data |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |