Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0965 GPa | 14.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 9002 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Flexural Modulus | 0.0965 GPa | 14.0 ksi | ASTM D790 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flexural Modulus | 0.0965 GPa | 14.0 ksi | ASTM D790 |
Ecomass® 4703ZD84 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica.. |
|||
Flexural Modulus | 0.0965 GPa | 14.0 ksi | 2% Secant; ASTM D638 |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |