Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.60 GPa | 1390 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
Quantum Composites QC-2150LD NT 25% Fiberglass Reinforced Phenolic SMC QC-2150LD NT (126-40-50) is a fiberglass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150LD NT (126-40-50) is.. |
|||
Flexural Modulus | 9.58 GPa | 1390 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications... |
|||
Flexural Modulus | 9.58 GPa | 1390 ksi | Crosswise; ASTM D-790 |
Glastic 1130 Angles, Channels, and Structural Shapes Information provided by Glastic Corporation |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
Grupo Repol Dinalon® A1S25 G45 H PA66 45% Glass Fiber, Heat Stabilized Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 9.58 GPa | 1390 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1130 FW Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applicati.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF008 Acetal Copolymer (Europe-Africa-Middle East) LNP* THERMOCOMP* KF008 is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PF0069 PA 6 (Europe-Africa-Middle East) LNP* STARFLAM* PF0069 is a compound based on PA 6 resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WC003 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC003 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.55 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp ZF008 PPO LNP* Thermocomp* ZF008 is a compound based on Modified PPO containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Flexural Modulus | 9.59 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
Plenco 4466 Phenolic, Granular, Transfer Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178-93 |
Wellman Wellamid® GF33-66 22LH-NBK1 Nylon 66, 33% Glass Fiber Reinforced, General Purpose Grade All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178-93 |
Wellman Wellamid® GF33A099-HRBK Nylon 66, 33% Glass Fiber Reinforced, Hydrolysis Resistant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
E-Polymers Tekaster® F615GM , 40% GF/MF Reinforced PET 40% GF/MF Reinforced, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 425 Polyester - PBT, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Flexural Modulus | 9.55 GPa @Temperature 120 °C |
1390 ksi @Temperature 248 °F |
ASTM D790 |
LATI LARTON G/50 50% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Flexural Modulus | 9.60 GPa | 1390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East) LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified. |