Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.951 GPa | 138 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.950 GPa @Temperature 23.0 °C |
138 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYten HDPE S801 HDPE, Good Abrasion Resistance, Excellent Sliding Properties Information provided by Polykemi AB |
|||
Flexural Modulus | >= 0.950 GPa | >= 138 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4240G (EP2S29B) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | >= 0.950 GPa | >= 138 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4341S Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Rotational Molded; ASTM D790 |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Flexural Modulus | >= 0.950 GPa | >= 138 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4340S (EP2H49G) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GD 5150 K HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.951 GPa | 138 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber. |
|||
Flexural Modulus | 0.953 GPa | 138 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB 68 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 802 Polypropylene Random Copolymer Applications include injection molding and extrusion. Basic stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com.. |
|||
Flexural Modulus | 0.953 GPa | 138 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.953 GPa | 138 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3702 Clarified Copolymer Polypropylene DescriptionPolyfort® PP 3702 is a clarified copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ISO 178 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 393 Ionomer DescriptionFormion® FI 393 is a 10% glass fiber reinforced, injection molding grade Ionomer, which has been formulated for scratch resistance, low CLTE, and impact. Formion F1 393U is UV stabilized.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | cond; ISO 178 |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Flexural Modulus | 0.952 GPa | 138 ksi | UNI EN ISO 14125: 2000 |
CRP Technology Windform® FX Polyamide Composite Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive.. |
|||
Flexural Modulus | 0.952 GPa | 138 ksi | |
Dow HDPE 38152M High Density Polyethylene DOW HDPE 38152M resin is a medium molecular weight distribution copolymer designed to offer good impact strength and stress crack resistance with excellent toughness. This resin has excellent proces.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | SAE J949 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.950 GPa | 138 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Flexural Modulus | >= 0.951 GPa | >= 138 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 0.950 GPa @Temperature 23.0 °C |
138 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |