Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.828 GPa | 120 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 0710 C Brown Polypropylene Data provided by Multibase. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | Tangent; ASTM D790 |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | >= 0.827 GPa | >= 120 ksi | ASTM D790 |
Niche Polymer PPCM10BK Copolymer PP Information provided by Niche Polymer |
|||
Flexural Modulus | 0.828 GPa | 120 ksi | ISO 178/1A |
Radici Heraflex® E 7722 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. High Modulus, Nominal Shore D/15s 69. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
(discontinued **) Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 0.827 - 1.93 GPa | 120 - 280 ksi | Average value: 1.49 GPa Grade Count:92 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PP2-1005ARX Biocompatible, Antimicrobial Polypropylene Random Copolymer A biocompatible approx. 10 melt Polypropylene random copolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information prov.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
Techmer ES HiFill FR® PP CO FR-N Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.825 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D882 |
A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | 1% secant; ASTM D790 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | 2% secant; ASTM D790 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | at 1% secant; ASTM D790 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | at 1% secant; ASTM D790 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | 1% secant; ASTM D790 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | 1% secant; ASTM D790 |
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good tou.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D882 |
A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | 2% secant; ASTM D790 |
A. Schulman LP544-01 High-Density Copolymer Polyethylene DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
Eastman Tenite 485E3720023 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | 2% Secant; ASTM D790 |
Chevron Phillips Marlex® H525 High Density Polyethylene, Pressure Pipe Grade This high performance PE 4710 HDPE is tailored for demanding pressure pipe applications that require:Good long-term hoop strengthGood resistance to slow crack growthExcellent resistance to slumpAddi.. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D790 |
Diamond Polymers NPP11-0242 Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 0.827 GPa | 120 ksi | ASTM D882 |
A. Schulman LP477-01 High-Density Polyethylene DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph.. |
|||
Flexural Modulus | 0.830 GPa | 120 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |