Mechanical Properties Metric English Comments
Flexural Modulus 0.7040 GPa
102.1 ksi
2% Secant; 12.5 mm/min; ASTM D790
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p..