Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0730 GPa | 10.6 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 9002 B BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.0731 GPa | 10.6 ksi | ASTM D790 |
Spartech Weather-Pro G Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |