Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00800 - 0.0100 GPa | 1.16 - 1.45 ksi | ISO 178 |
PolyOne Bergadur™ PB400 G30 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Flexural Modulus | 0.00800 - 2.50 GPa @Temperature -40.0 - 100 °C |
1.16 - 363 ksi @Temperature -40.0 - 212 °F |
Average value: 0.758 GPa Grade Count:10 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 0.00800 - 11.0 GPa | 1.16 - 1600 ksi | Average value: 8.29 GPa Grade Count:234 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Flexural Modulus | 0.00800 GPa | 1.16 ksi | ASTM D638 |
Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 29 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 29 MA 03 is a polyme.. |