Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.01 - 9.20 GPa | 1160 - 1330 ksi | Average value: 8.60 GPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 0.600 - 9.20 GPa | 87.0 - 1330 ksi | Average value: 2.60 GPa Grade Count:88 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |