Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.686 - 7.11 GPa | 99.6 - 1030 ksi | Average value: 2.10 GPa Grade Count:299 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |