Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.50 - 6.50 GPa | 798 - 943 ksi | ISO 178 |
Perstorp Compounds Aminel FX Melamine Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp .. |
|||
Flexural Modulus | 4.50 - 6.50 GPa | 653 - 943 ksi | ASTM D790 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Modulus | 4.50 - 6.50 GPa | 653 - 943 ksi | ASTM D790 |
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |