Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.65 - 6.21 GPa | 240 - 900 ksi | Average value: 1.94 GPa Grade Count:18 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Flexural Modulus | 3.20 - 6.21 GPa | 464 - 900 ksi | Average value: 5.01 GPa Grade Count:25 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Flexural Modulus | 1.14 - 6.21 GPa | 165 - 900 ksi | Average value: 3.16 GPa Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |