Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.345 - 5.85 GPa | 50.0 - 848 ksi | Average value: 2.37 GPa Grade Count:18 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |