Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0150 - 3.09 GPa | 2.18 - 448 ksi | Average value: 0.408 GPa Grade Count:63 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |