Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.21 - 28.3 GPa | 900 - 4100 ksi | Average value: 13.8 GPa Grade Count:44 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Modulus | 7.58 - 28.3 GPa | 1100 - 4100 ksi | Average value: 17.0 GPa Grade Count:32 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |