Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.60 - 26.0 GPa | 957 - 3770 ksi | Average value: 13.7 GPa Grade Count:52 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Flexural Modulus | 10.0 - 26.0 GPa | 1450 - 3770 ksi | Average value: 13.3 GPa Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Graphite Filled". Each property range of values reported is minimum and maxim.. |