Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 20.0 - 22.0 GPa | 2900 - 3190 ksi | ISO 178 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Flexural Modulus | 20.0 - 22.0 GPa | 2900 - 3190 ksi | ISO 178 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Flexural Modulus | 18.0 - 22.0 GPa | 2610 - 3190 ksi | Injection; ISO 178 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Flexural Modulus | 9.00 - 22.0 GPa | 1310 - 3190 ksi | Average value: 14.0 GPa Grade Count:6 |
Overview of materials for Phenolic/Glass Fiber SMC This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Modulus | 9.30 - 22.0 GPa | 1350 - 3190 ksi | Average value: 14.4 GPa Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Flexural Modulus | 17.0 - 22.0 GPa | 2470 - 3190 ksi | Longitudinal |
Goodfellow Polyaramid/Vinylester Composite Tube or Rod Information provided by Goodfellow. |
|||
Flexural Modulus | 18.0 - 22.0 GPa | 2610 - 3190 ksi | Injection; ISO 178 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |