Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.55 - 2.55037 GPa @Temperature 149 - 150 °C |
370 - 369.906 ksi @Temperature 300 - 302 °F |
Average value: 2.55 GPa Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Unfilled |