Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.152 - 2.21 GPa | 22.0 - 320 ksi | Average value: 0.366 GPa Grade Count:18 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |