Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.0 - 19.0 GPa | 2320 - 2760 ksi | Injection and Compression; ISO 178 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Flexural Modulus | 16.0 - 19.0 GPa | 2320 - 2760 ksi | Injection; ISO 178 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Flexural Modulus | 11.7 - 19.0 GPa | 1700 - 2760 ksi | Average value: 14.6 GPa Grade Count:12 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Flexural Modulus | 7.53 - 19.0 GPa | 1090 - 2760 ksi | Average value: 11.5 GPa Grade Count:3 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 6.70 - 19.0 GPa | 972 - 2760 ksi | Average value: 8.15 GPa Grade Count:19 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 7.20 - 19.0 GPa @Temperature -40.0 - 80.0 °C |
1040 - 2760 ksi @Temperature -40.0 - 176 °F |
Average value: 13.4 GPa Grade Count:1 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Flexural Modulus | 14.0 - 19.0 GPa | 2030 - 2760 ksi | ISO 178 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |