Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.50 - 10.5 GPa | 943 - 1520 ksi | Average value: 8.61 GPa Grade Count:15 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Flexural Modulus | 4.80 - 10.5 GPa | 696 - 1520 ksi | Average value: 8.22 GPa Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 8.60 - 10.5 GPa | 1250 - 1520 ksi | Average value: 9.44 GPa Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |