Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.238 - 10.4 GPa | 34.5 - 1510 ksi | Average value: 2.79 GPa Grade Count:22 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Flexural Modulus | 8.16 - 10.4 GPa | 1180 - 1510 ksi | Average value: 9.12 GPa Grade Count:10 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |