Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.20 - 1.50 GPa | 174 - 218 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8430 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Modulus | 1.20 - 1.50 GPa | 174 - 218 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8530_Gray60 Polypropylene-like Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | 1.30 - 1.50 GPa | 189 - 218 ksi | ASTM D790 |
Loxim 800 00 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |